產(chǎn)品參數(shù)
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
性能 | 模收縮 | 2.2-2.4 | % | ||
比重 | ASTM D-792 | 1.41 | |||
吸水量 | 浸漬平衡點 | ASTM D-570 | 0.80 | % | |
吸水量 | 50%相對濕度 | ASTM D-570 | 0.20 | % | |
吸水量 | 24小時浸漬 | ASTM D-570 | 0.26 | % | |
撓曲系數(shù) | 122℃ | ASTM D-790 | 755 | MPa | |
壓縮應(yīng)力 | 23℃,10%變形 | ASTM D-695 | 123 | MPa | |
IZOD沖擊試驗 | 23℃ | ASTM D-256 | 81 | j/m | |
熔點 | ASTM D-2133 | 175 | ℃ | ||
撓曲疲勞忍耐限度 | 50%RH,23℃,106周期 | ASTM D-671 | 31 | MPa | |
洛氏硬度 | ASTM D-785 | 94 | M scale | ||
撓曲系數(shù) | 100℃ | ASTM D-790 | 1030 | % | |
破裂點拉伸變形量 | 70℃ | ASTM D-638 | 220 | % | |
撓曲系數(shù) | 23℃ | ASTM D-790 | 3090 | MPa | |
抗電弧 | 3.1mm | ASTM D-495 | 220 | sec | |
壓縮應(yīng)力 | 23℃,1%變形 | ASTM D-695 | 35 | MPa | |
破裂點拉伸變形量 | 122℃ | ASTM D-638 | >260 | % | |
彈性系數(shù) | 23℃ | ASTM D-638 | 3360 | MPa | |
容積電阻率 | 23℃,0.2%含水量 | ASTM D-257 | 1×1015 | Ω.cm | |
洛氏硬度 | ASTM D-785 | 120 | R scale | ||
破裂點拉伸變形量 | 23℃ | ASTM D-638 | 35 | % | |
IZOD沖擊試驗 | 無缺口23℃ | ASTM D-256 | 2160 | j/m | |
熱畸變溫度 | 1.8MPa | ASTM D-648 | 136 | MPa | |
線性熱膨脹系數(shù) | -40~29℃ | ASTM D-696 | 13.7 | 10-5m/m℃ | |
撓曲變形強度 | 23℃ | ASTM D-790 | 97 | MPa | |
拉伸強度 | 23℃ | ASTM D-638 | 69 | MPa | |
IZOD沖擊試驗 | 缺口-40℃ | ASTM D-256 | 66 | j/m | |
抗剪強度 | 23℃ | ASTM D-732 | 66 | MPa |