產(chǎn)品參數(shù)
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
物理性能 | 成型收縮率 | 縱向 | ASTM D-570 | 1.8-2.1 | % | |
橫向 | ASTM D-570 | - | % | |||
機(jī)械性能 | 拉伸屈服應(yīng)力 | 122℃ | ASTM D-638 | 21 | MPa | |
彎曲強(qiáng)度 | 23℃ | ASTM D-790 | 105 | MPa | ||
彎曲模量 | 100℃ | ASTM D-790 | 900 | MPa | ||
懸臂梁缺口沖擊強(qiáng)度 | 23℃ | ASTM D-256 | 75 | J/m | ||
拉伸斷裂應(yīng)變 | 70℃ | ASTM D-638 | >60 | % | ||
彎曲強(qiáng)度 | -55℃ | ASTM D-790 | 177 | MPa | ||
洛氏硬度 | ASTM D-785R | 121 | ||||
拉伸屈服應(yīng)力 | 100℃ | ASTM D-638 | 28 | MPa | ||
彎曲模量 | -55℃ | ASTM D-790 | 4330 | MPa | ||
彎曲強(qiáng)度 | 122℃ | ASTM D-790 | 25 | MPa | ||
懸臂梁無(wú)缺口沖擊強(qiáng)度 | 23℃ | ASTM D-256 | >1500 | J/m | ||
拉伸斷裂應(yīng)變 | 23℃ | ASTM D-638 | 56 | % | ||
彎曲模量 | 23℃ | ASTM D-790 | 3270 | MPa | ||
彎曲模量 | 70℃ | ASTM D-790 | 1480 | MPa | ||
彎曲強(qiáng)度 | 70℃ | ASTM D-790 | 54 | MPa | ||
彎曲強(qiáng)度 | 100℃ | ASTM D-790 | 35 | MPa | ||
壓縮應(yīng)力 | 23℃,10%變形 | ASTM D-695 | 105 | MPa | ||
洛氏硬度 | ASTM D-785M | 87 | ||||
拉伸斷裂應(yīng)變 | 100℃ | ASTM D-638 | >60 | % | ||
拉伸斷裂應(yīng)變 | 122℃ | ASTM D-638 | >60 | % | ||
拉伸屈服應(yīng)力 | -55℃ | ASTM D-638 | 109 | MPa | ||
拉伸斷裂應(yīng)變 | -55℃ | ASTM D-638 | 29 | % | ||
懸臂梁缺口沖擊強(qiáng)度 | 23℃ | ASTM D-256 | 68 | J/m | ||
彎曲模量 | 122℃ | ASTM D-790 | 630 | MPa | ||
壓縮應(yīng)力 | 23℃,1%變形 | ASTM D-695 | 28 | MPa | ||
拉伸屈服應(yīng)力 | 23℃ | ASTM D-638 | 71 | MPa | ||
剪切強(qiáng)度 | 23℃ | ASTM D-732 | 64 | MPa | ||
拉伸屈服應(yīng)力 | 70℃ | ASTM D-638 | 45 | MPa | ||
電氣性能 | 體積電阻率 | 23℃ | ASTM D-257 | 1015 | Ωm | |
熱性能 | 融解溫度 | ASTM D-2133 | 175 | ℃ | ||
熱變形溫度 | 0.46MPa | ASTM D-648 | 168 | ℃ | ||
熱變形溫度 | 1.82MPa | ASTM D-648 | 125 | ℃ | ||
其它性能 | 比重 | 23℃ | ASTM D-792 | 1.42 | MPa | |
吸水率 | ASTM D-570 | 0.36 | ||||
線性膨脹系數(shù) | -40~29 | ASTM D-696 | 10.1 | 10-5m/m℃ | ||
線性膨脹系數(shù) | 29~60 | ASTM D-696 | 12.3 | 10-5m/m℃ | ||
線性膨脹系數(shù) | 60~104 | ASTM D-696 | 14.1 | 10-5m/m℃ | ||
線性膨脹系數(shù) | 104~150 | ASTM D-696 | 15.5 | 10-5m/m℃ |