廠家(產(chǎn)地):美國杜邦 | 加工級別:注塑級 | 牌號:5526 |
類型:標準料 | 銷售方式:品牌經(jīng)銷 | 特性級別:阻燃級 |
產(chǎn)品參數(shù)
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能
|
比重 | ASTM D792 | 1.20 |
g/cm3;
|
|
ISO 1183 | 1.19 |
g/cm3;
|
|||
熔流率 |
220℃/2.16 kg
|
ASTM D1238 | 18 |
g/10 min
|
|
溶化體積流率 | 220℃/2.16 kg | ISO 1133 | 16.0 |
cm3;/10min
|
|
收縮率 | 流動 | ASTM D955 | 1.4 |
%
|
|
橫向流量: 2.00 mm
|
ISO 294-4 | 1.4 | % | ||
流量: 2.00 mm
|
ISO 294-4 | 1.4 | % | ||
吸水率 |
23℃, 24 hr
|
ASTM D570,ISO 62 | 0.50 | % | |
23℃, 24 hr | ISO 62 | 0.60 | % | ||
飽和, 23℃ | ISO 62 | 0.60 | % | ||
平衡, 23℃, 50% RH
|
ISO 62 | 0.20 | % | ||
硬度 |
支撐 D
|
ASTM D2240,ISO 868 | 55 | ||
支撐 D,15秒
|
ISO 868 | 51 | |||
機械性能 |
拉伸模量 | 23℃ | ISO 527-2 | 188 |
MPa
|
拉伸應力 |
屈服, 23℃
|
ASTM D638 | 14.0 |
MPa
|
|
斷裂, 23℃
|
ISO 527-2 | 40.0 |
MPa
|
||
斷裂, 23℃ | ISO 527-2 | 44.0 |
MPa
|
||
5.0% 應變, 23℃
|
ASTM D638 | 6.90 |
MPa
|
||
10%應變, 23℃
|
ASTM D638 | 10.3 |
MPa
|
||
拉伸應變 | 屈服, 23℃ | ISO 527-2 | 37 |
%
|
|
斷裂, 23℃ | ASTM D638 | 550 |
%
|
||
斷裂, 23℃ | ISO 527-2 | 500 | % | ||
斷張率 | 23℃ | ISO 527-2 | 800 |
%
|
|
-40℃ | ASTM D790,ISO 178 | 760 |
MPa
|
||
23℃ | ASTM D790 | 207 |
MPa
|
||
彎曲模量 | 100℃ | ASTM D790 | 110 |
MPa
|
|
23℃ | ISO 178 | 200 |
MPa
|
||
100℃ | ISO 178 | 100 |
MPa
|
||
Tensile Stress |
23℃, 5% Strain
|
ISO 527-2 | 6.90 | MPa | |
23℃, 10% Strain
|
ISO 527-2 | 11.0 | MPa | ||
簡支梁缺口沖擊強度 | -40℃ | ISO 179/1eA | 150 |
kJ/m2;
|
|
-30℃ | ISO 179/1eA | 90 | |||
23℃ | ISO 179/1eA | 無斷裂 | |||
簡支梁缺口沖擊強度 | -30℃ | ISO 179/1eU | 無斷裂 | ||
23℃ | ISO 179/1eU | 無斷裂 | |||
懸壁梁缺口沖擊強度 | -40℃ | ASTM D256 | 130 |
J/m
|
|
23℃ | ASTM D256 | 無斷裂 | |||
-40 | ISO 8256 | 120 |
kJ/m2;
|
||
拉伸沖擊強度 | 23℃ | ISO 8256 | 200 |
kJ/m2;
|
|
熱性能 |
熱變形溫度 | 0.45 MPa, 未退火 | ASTM D648 | 90.0 | ℃ |
0.45 MPa, 未退火 | ISO 75-2/B | 65.0 | ℃ | ||
1.8 MPa, 未退火
|
ASTM D648 | 49.0 | ℃ | ||
1.8 MPa, 未退火
|
ISO 75-2/B | 45.0 | ℃ | ||
脆化溫度 | ISO 974 | -98.0 | ℃ | ||
玻璃轉化溫度 | ISO 11357-2 | -20.0 | ℃ | ||
熔融溫度 2 | ISO 11357-3,ASTM D3418 | 203 | ℃ | ||
線形膨脹系數(shù) | 流動: -40 到 23℃ | ASTM E831,ISO 11359-2 | 0.00021 |
cm/cm/℃
|
|
流動: 23 到 55℃ | ASTM E831,ISO 11359-2 | 0.00019 | cm/cm/℃ | ||
流動: 55 到 120℃ | ASTM E831,ISO 11359-2 | 0.00016 | cm/cm/℃ | ||
流動: 23 到 55℃
|
ISO 11359-2 | 0.00020 | cm/cm/℃ | ||
橫向: -40 到 23℃ | ASTM E831,ISO 11359-2 | 0.00021 | cm/cm/℃ | ||
橫向: 23 到 55℃ | ASTM E831,ISO 11359-2 | 0.00017 | cm/cm/℃ | ||
橫向: 55 到 120℃ | ASTM E831,ISO 11359-2 | 0.00011 | cm/cm/℃ | ||
橫向: 23 到 55℃
|
ISO 11359-2 | 0.00019 | cm/cm/℃ | ||
電氣性能 |
表面電阻率 | IEC 60093 |
2.0E+15
|
ohms
|
|
體積電阻率 | IEC 60093 |
4.0E+13
|
ohm·cm
|
||
介電強度 |
23℃, 1.91 mm 3
|
ASTM D149 | 17 | kV/mm | |
23℃ | IEC 60243-1 | 20 |
kV/mm
|
||
介電常數(shù) |
23℃, 1.91 mm, 100 Hz
|
ASTM D150 | 4.50 | ||
23℃, 1.91 mm, 1 kHz
|
ASTM D150 | 4.50 | |||
23℃, 1.91 mm, 1 MHz
|
ASTM D150 | 4.20 | |||
23℃, 100 Hz
|
IEC 60250 | 4.90 | |||
23℃, 1 Hz
|
IEC 60250 | 4.60 | |||
耗散因數(shù) |
23℃, 1.91 mm, 100 Hz
|
ASTM D150 | 0.0060 | ||
23℃, 1.91 mm, 1Hz
|
ASTM D150 | 0.0090 | |||
23℃, 1.91 mm, 1Hz
|
ASTM D150 | 0.040 | |||
23℃, 100 Hz
|
IEC 60250 | 0.0090 | |||
23℃, 1 Hz
|
IEC 60250 | 0.038 | |||
漏電起痕指數(shù) | IEC 60112 |
> 600
|
V
|
||
UL 阻燃等級 | 1.50 mm | UL 94 | HB | ||
3.00 mm
|
UL 94 | HB | |||
可燃性等級 | 1.50 mm | IEC 60695-11-10, -20 |
HB
|
||
3.00 mm
|
IEC 60695-11-10, -20 | HB | |||
極限氧指數(shù) | ISO 4589-2 | 21 |
%
|
||
RTI Str | 1.50 mm | UL 746 | 50.0 | ℃ | |
3.00 mm
|
UL 746 | 50.0 | ℃ | ||
RTI Imp | 1.50 mm | UL 746 | 50.0 | ℃ | |
3.00 mm | UL 746 | 50.0 | ℃ | ||
RTI Elec | 1.50 mm | UL 746 | 50.0 | ℃ | |
3.00 mm | UL 746 | 50.0 | ℃ | ||
其它 | 干燥溫度 | 100 | ℃ | ||
干燥時間 |
2.0 到 3.0
|
hr | |||
建議的大水分含量 |
< 0.080
|
% | |||
Melt Temperature, Optimum |
Injection Molding |
230
|
℃ | ||
模具溫度 |
45.0 到 55.0
|
℃ | |||
Mold Temperature, Optimum |